摘要 PROBLEM TO BE SOLVED: To provide an active material and an electrode which have sufficient charge and discharge cycle characteristics and high safety at the time of high-temperature reservation and a nailing test, and a manufacturing method of these.SOLUTION: The manufacturing method of the active material is provided with a process in which lithium-containing metal oxide particles are contacted to aqueous solution which contains a metal fluoro-complex and lithium salt and of which concentration of boric acid is 0.01 M or less. The manufacturing method of the electrode is provided with a process in which the aqueous solution which contains a metal fluoro-complex and lithium salt with the concentration of boric acid of 0.01 M or less is made to contact an electrode having an active material layer containing lithium-containing metal oxide particles, a conductive assistant, and a binder.
申请公布号 JP5510002(B2) 申请公布日期 2014.06.04
申请号 JP20100082837 申请日期 2010.03.31
申请人 发明人
分类号 H01M4/525;H01G11/06;H01G11/22;H01G11/30;H01G11/46;H01M4/131;H01M4/1391;H01M4/485;H01M4/505 主分类号 H01M4/525
代理机构 代理人
主权项
地址