摘要 <p>A graphite film showing an extremely low average tearing force is more likely to suffer from various kinds of defects, such as splitting, winding deviation, wrinkling, and poor dimensional accuracy, in a step of producing the graphite film and in a step of processing the graphite film. However, these defects can be prevented by using a graphite film that satisfies the following requirements: 1) having an average tearing force of not more than 0.08 N as determined by Trouser tear method in accordance with JIS K7128; and 2) having sag of not less than 5 mm and not greater than 80 mm as determined by a method of film windability evaluation in accordance with JIS C2151.</p>