摘要 |
Electrostatic latent image developing toner includes at least a binder resin and a releasing agent. In the electrostatic latent image developing toner, a maximum thermal expansion coefficient difference (Swmax−Srmax), which is a difference between a maximum value (Swmax) of a thermal expansion coefficient of the releasing agent and a maximum value (Srmax) of a thermal expansion coefficient of the binder resin, is 1 or more, and a temperature at which the thermal expansion coefficient of the releasing agent reaches a maximum is 60° C. or more to 75° C. or less. |