发明名称 |
AMORPHOUS METAL COMPOSITE AND METHOD FOR PRODUCING THE SAME |
摘要 |
PROBLEM TO BE SOLVED: To provide an amorphous metal composite and a method for producing the same.SOLUTION: An alloy is heated to a high temperature higher than the liquidus temperature. When the melt at a high temperature is cooled, dendrites are formed in the melt by the density distribution of the alloy. When the remaining melt is cooled to a low temperature lower than the glass transition temperature, the melt is solidified into the amorphous state and a two-phase structure in which crystalline particles are present in an amorphous metal matrix is formed. The ductile metal particles have a particle diameter of 0.1 to 15 μm and a particle spacing of 0.1 to 20 μm, preferably a particle diameter of 0.5 to 8 μm and a particle spacing of 1 to 10 μm. The volume percentage of particles is 5 to 50% and preferably 15 to 35%. The dendrites of the ductile metal phase in the amorphous matrix can be oriented by directional cooling. |
申请公布号 |
JP2014088622(A) |
申请公布日期 |
2014.05.15 |
申请号 |
JP20130257353 |
申请日期 |
2013.12.12 |
申请人 |
CALIFORNIA INST OF TECHNOLOGY |
发明人 |
HAYS CHARLES C;KIM CHOONG PAUL;JOHNSON WILLIAM L |
分类号 |
C22C16/00;C22C47/00;C22C9/00;C22C14/00;C22C25/00;C22C30/00;C22C33/00;C22C45/10;C22C49/02;C22C111/00;C22F1/00;C22F1/08;C22F1/16;C22F1/18 |
主分类号 |
C22C16/00 |