摘要 |
<p>Molding material (A) obtained by the polymerization of ethylene, exhibits a density of 0.940-0.96 g/cm3>, melt index of 0.5-10 g/10minutes, molar mass distribution of 3-20, ramification value of 1000C is 0.1-10, and weight average molecular mass of 50000-150000 g/mol. Independent claims are included for: (1) an injection-molded body obtained from (A); and (2) screw value comprising (A).</p> |