摘要 The pressure-sensitive adhesive film or sheet of the present invention comprises an adhesive layer, which contains an ethylene-vinyl acetate copolymer the vinyl acetate content of which is between 7.5 and 20 mass% and an agent for imparting adhesion having a softening point that is between 95 and 150ºC as determined in accordance with the JISK2207-1996 ring-and-ball method and wherein when the total amount of ethylene-vinyl acetate copolymer and agent for imparting adhesion is 100 parts by mass, the content of agent for imparting adhesion is between 0.1 and 1.0 parts by mass.
申请公布号 JP5485476(B2) 申请公布日期 2014.05.07
申请号 JP20130524597 申请日期 2012.07.10
申请人 发明人
分类号 C09J7/00;B32B27/00;B32B27/18;B32B27/28;C09J7/02;C09J123/08;C09J131/04 主分类号 C09J7/00