<p>Described are: an active-energy-ray-curable composition (38) containing a phosphate ester compound of which an aqueous solution prepared by extracting with 50 mL of water per 1 g of the phosphate ester compound has a pH value of 6.5 to 7.5 at 25° C., wherein the value of (the concentration of phosphoric acid in the aqueous solution, expressed in mass ppm)×(the content of the phosphate ester compound in the active-energy-ray-curable composition, expressed in mass %) is 50 or less; and a process for producing a transparent film (40) which includes the active-energy-ray-curable composition (38) and in which a cured resin layer (44) having a fine uneven structure is formed on the surface of a base film (42).</p> |