发明名称 |
METHOD FOR PREPARING A TITANIUM AND NIOBIUM MIXED OXIDE BY SOLVOTHERMAL TREATMENT; ELECTRODE AND LITHIUM ACCUMULATOR COMPRISING SAID MIXED OXIDE |
摘要 |
This method for preparing a titanium and niobium mixed oxide comprises the following steps: -preparation of a titanium and niobium mixed oxide in amorphous form by solvothermal treatment of at least one titanium precursor and at least one niobium precursor; -mechanical crushing of the titanium and niobium mixed oxide obtained from the solvothermal treatment; -calcination of the mixed oxide obtained after crushing. |
申请公布号 |
WO2014060662(A1) |
申请公布日期 |
2014.04.24 |
申请号 |
WO2013FR52099 |
申请日期 |
2013.09.12 |
申请人 |
COMMISSARIAT A L'ENERGIE ATOMIQUE ET AUX ENERGIESALTERNATIVES |
发明人 |
BUANNIC, LUCIENNE;COLIN, JEAN-FRANÇOIS;DANIEL, LISE |
分类号 |
C01G33/00;H01M4/485 |
主分类号 |
C01G33/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|