发明名称 |
JOINT METHOD OF FERROUS MATERIAL AND POLYAMIDE RESIN, AND CONJUGATE |
摘要 |
PROBLEM TO BE SOLVED: To improve adhesive strength when a PA resin is coated on a ferrous material component (work-piece), and to make a PA resin hardly peel.SOLUTION: Concretely, a method of jointing a ferrous material and a polyamide resin includes: a step in which the ferrous material processed to a desired shape is cleaned; a step in which etching with heated sulphuric acid is performed on the ferrous material; a step in which the heated sulfuric acid etching processes a surface of the ferrous material to a rough surface in which holes of a 200 nm size are formed in a network; and a step in which the polyamide resin is melted to be jointed with the ferrous material. |
申请公布号 |
JP2014054836(A) |
申请公布日期 |
2014.03.27 |
申请号 |
JP20130166518 |
申请日期 |
2013.08.09 |
申请人 |
NST SEISAKUSHO:KK |
发明人 |
ISHII HIDEAKI;MATSUMOTO TAKASHI;SATO NOBUO |
分类号 |
B32B38/00;B29C65/64;B32B15/088 |
主分类号 |
B32B38/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|