发明名称 |
HIGH-STRENGTH, LOW-WARPING ELECTROLYTIC COPPER FOIL AND METHOD FOR PRODUCING SAME |
摘要 |
This electrolytic copper foil is characterized by the tensile strength in an ordinary state (hereinafter referred to as "ordinary state tensile strength") being 45-55 kgf/mm2, and the average amount of lift of the four 100 mm corners being no greater than 2 mm, and the tensile strength after heating for 60 minutes at 180°C (hereinafter referred to as "post-heating tensile strength") is at least 85% of the ordinary state tensile strength. The problem addressed by the present invention is to provide an electrolytic copper foil that has a high ordinary state tensile strength and post-heating tensile strength and a low amount of warping, particularly an electrolytic copper foil useful as a secondary battery anode collector. |
申请公布号 |
KR20140035524(A) |
申请公布日期 |
2014.03.21 |
申请号 |
KR20147003631 |
申请日期 |
2011.12.05 |
申请人 |
JX NIPPON MINING & METALS CORPORATION |
发明人 |
KOHIKI MICHIYA |
分类号 |
C25D1/04;H01M4/64;H01M4/66 |
主分类号 |
C25D1/04 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|