摘要 |
<p>The present invention improves efficiency of production. A method for manufacturing nickel is provided with a reduction step (S200) and a recovery step (S202). The reduction step (S200) has a nickel hydroxide mixture continuous transporting step (S210), a reducing agent continuous transporting step (S212), and a continuous manufacturing step (S214). The nickel hydroxide mixture continuous transporting step (S120) is a step for continuously transporting a mixture of nickel hydroxide powder and a fluidization liquid through a tube. The reducing agent continuous transporting step (S212) is a step for continuously transporting a reducing agent. The continuous manufacturing step (S214) is a step for manufacturing a fluid including nickel by continuously mixing the reducing agent, the nickel hydroxide powder, and supercritical water or subcritical water.</p> |