发明名称 |
PRODUCTION METHOD OF SINTERED ORE |
摘要 |
PROBLEM TO BE SOLVED: To provide a production method of sintered ore by which decrease in productivity and rise in production cost caused by change in property of coke breeze and anthracite as a coagulation material, and change or the like in particle size composition accompanying the change can be suppressed.SOLUTION: Before and after a brand and/or a ratio of a carbonaceous material included in a coagulation material is changed, calorific power derived from particles of a particle diameter of at most 1 mm of the coagulation material after the change is maintained same as calorific power derived from particles of a particle diameter of at most 1 mm before the change. It is desirable that deterioration in a basic unit of the coagulation material is suppressed while calorific powers derived from particles of a particle diameter of at most 1 mm before and after the change are maintained to become same by adjusting a particle ratio of particles of a particle diameter of at most 1 mm of the coagulation material. |
申请公布号 |
JP2014040618(A) |
申请公布日期 |
2014.03.06 |
申请号 |
JP20120182248 |
申请日期 |
2012.08.21 |
申请人 |
NIPPON STEEL & SUMITOMO METAL |
发明人 |
SASAKI TAKAHIRO;WATANABE KEI;MASUTANI YASUYUKI |
分类号 |
C22B1/16 |
主分类号 |
C22B1/16 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|