摘要 |
The present invention relates to a alkali-silica reaction suppression waste glass aggregate mixed concrete composition, a method for producing the same, a concrete structure including the same, more specifically , and to a mixed concrete composition for suppressing alkali-silica reaction by using waste aggregate with the average granularity 1 -5 mm and including glass polishing sludge with the average granularity 5 -20μm. [Reference numerals] (AA) Section;(BB) 3 days;(CC) 6 days;(DD) 9 days;(EE) 12 days;(FF) 14 days;(GG) 16 days;(HH) 20 days;(II) 24 days;(JJ) 28 days;(KK) 30 days;(LL) 40 days;(MM) 50 days |