发明名称 |
CERAMIC COMPOSITION FOR MAKING LIGHT BRICK |
摘要 |
FIELD: chemistry.SUBSTANCE: ceramic composition for making light brick contains ash-slag material and interslate clay, containing the following, wt %: SiO- 41.3; AlO- 14.4; FeO- 6.8; CaO - 9.2; MgO - 2.5; RO - 4.1; loss on ignition - 20.2, with the following ratio of components, wt %: interslate clay - 50-70; ash-slag material - 30-50.EFFECT: high frost resistance and low heat conductivity of articles.3 tbl |
申请公布号 |
RU2508269(C2) |
申请公布日期 |
2014.02.27 |
申请号 |
RU20120100791 |
申请日期 |
2012.01.11 |
申请人 |
FEDERAL'NOE GOSUDARSTVENNOE BJUDZHETNOE OBRAZOVATEL'NOE UCHREZHDENIE VYSSHEGO PROFESSIONAL'NOGO OBRAZOVANIJA "SAMARSKIJ GOSUDARSTVENNYJ AEHROKOSMICHESKIJ UNIVERSITET IMENI AKADEMIKA S.P. KOROLEVA (NATSIONAL'NYJ ISSLEDOVATEL'SKIJ UNIVERSITET)" (SGAU) |
发明人 |
ABDRAKHIMOVA ELENA SERGEEVNA;ROSHCHUPKINA IRINA JUR'EVNA;KOLPAKOV ALEKSANDR VIKTOROVICH;ABDRAKHIMOV VLADIMIR ZAKIROVICH |
分类号 |
C04B33/135 |
主分类号 |
C04B33/135 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|