发明名称 SEALANT COMPOSITION, PREFORMED SEALANT AND SEALANT CONSTRUCTION METHOD USING THE SAME
摘要 The present invention is, as a joint filler composition comprising: 50-80 wt% of petroleum asphalt, 5-25 wt% of a flow agent, 1-25 wt% a polymer modifier, 0.1-2 wt% of a heat stabilizer, poured joint filler using the same, molded joint filler, and a joint construction method, can be firmly attached to a junction unit between concrete and asphalt of a road pavement, has an excellent construct ability, heat resistance, and flow resistance, effectively responds to external stress, and improves durability by blocking retained water in package or by guiding drainage or low noise, retained water in porous package towards the drain outlet.
申请公布号 KR101357760(B1) 申请公布日期 2014.02.05
申请号 KR20130095394 申请日期 2013.08.12
申请人 KOREA PETROLEUM INDUSTRLAL CO., LTD. 发明人 YANG, JAE BONG;LEE, JIN HO;LEE, KWANG HO;KIM, YONG CHEOL
分类号 E01C11/02;C08L95/00 主分类号 E01C11/02