PROBLEM TO BE SOLVED: To provide a coated molding with a fair balance between impact resistance and scratch resistance before coating, and with a fair balance between coating clarity and film adhesion after coating.SOLUTION: In a molding which is composed of a thermoplastic resin (C) including a rubbery copolymer (A) formed by copolymerizing a rubber constituent with a vinyl cyanide monomer and another monomer and a copolymer (B) formed by copolymerizing a vinyl cyanide monomer with another monomer, 1) the copolymer (B) includes a copolymer (B1) and a copolymer (B2), 2) two phases respectively originating from two copolymers (B1) and (B2) are recognized in a morphology obtained via observation of the molding with a transmission electron microscope (TEM), and a rubbery copolymer including a rubber constituent with a volume average particle size of 50-1,000 nm exists in both phases of the copolymer (B), and 3) the molding has a coating applied thereto. |