Fire-resistant coating material ADINA comprising ammonium polyphosphate in the amount of 5 to 50% w/w, pentaerythritol in the amount of 6 to 33% w/w, melamine in the amount of 4 to 22% w/w, binder based on polyvinylacrylate dispersion in the amount of 10 to 16.3% w/w, plasticizer based on diisononylphthalate in the amount of 2.3 to 3.5% w/w, talc in the amount of 3 to 10% w/w, stabilizer (preservative) based on 4-chloro-3-methylphenol in the amount of 0.15 to 0.25% w/w, and water in the amount of 13.5 to 17% w/w. |