摘要 |
A rubber composition comprises a diene rubber including not less than 30% by weight of a modified conjugated diene polymer rubber and, per 100 parts by weight of the diene rubber, from 1 to 25 parts by weight of a tackifying resin, and from 25 to 80 parts by weight of a filler comprising not less than 50% by weight of silica. The modified conjugated diene polymer rubber has a terminal modified group comprising a functional group that interacts with silica. In the modified conjugated diene polymer rubber, aromatic vinyl unit content is from 38% to 48% by weight, vinyl unit content is from 20% to 35%, weight-average molecular weight is from 600,000 to 1,000,000, and glass transition temperature is from -22 to -32� C. A glass transition temperature of the tackifying resin is from 50 to 110� C. higher than the glass transition temperature of the modified conjugated diene polymer rubber. |