摘要 |
<p>Provided are a warming and heat storage fiber, a method for preparing a textile fiber that rapidly warms up and stores heat when exposed to light, and a textile that rapidly warms up and stores heat when exposed to light. The warming and heat storage fiber comprises: a conventional textile fiber and a nanometer unit accounting for 0.1-3% (part by weight) of a total weight. The nanometer unit comprises microparticles with a particle size of 300-8000 nanometers. The microparticles comprise at least a mixture of at least two of silicon, titanium, and antimony.</p> |