摘要 |
Resins suitable for rotomolded articles comprise a bimodal polyethylene copolymer comprising from 0.1 to 5 weight % of one or more C6-8 alpha olefins and the balance ethylene, comprising from 20 to 50 weight % of a higher molecular weight polymer component having an Mw greater than 120,000 and correspondingly from 80 to 50 weight % of a lower molecular weight polymer component having an Mw less than 100,000 having a density greater than 0.942 g/cc [but less than 0.965 g/cc] and a bent strip ESCR as determined by ASTM D 1693 in 100% Igepal® CO-630 (ethoxylated nonylphenols) for conditions A and B of greater than 1000 hours. The resulting articles have a very good balance of properties and significant ESCR.
|