摘要 PROBLEM TO BE SOLVED: To obtain a glass composition for sealing having a low thermal expansion coefficient and good flowability at a temperature of not higher than 600&deg;C while satisfying environmental requirements in recent years. SOLUTION: The glass composition for sealing contains, by mass, 60 to &lt;77% of Bi<SB>2</SB>O<SB>3</SB>, 5 to 20% of B<SB>2</SB>O<SB>3</SB>, 3 to 15% of ZnO, and &gt;1 to 7% of SiO<SB>2</SB>as glass components, and has a thermal expansion coefficient of &le;100&times;10<SP>-7</SP>/&deg;C within a temperature range of 30-300&deg;C. COPYRIGHT: (C)2009,JPO&amp;INPIT
申请公布号 JP5344363(B2) 申请公布日期 2013.11.20
申请号 JP20080116597 申请日期 2008.04.28
申请人 发明人
分类号 C03C8/04;H01J61/30 主分类号 C03C8/04