摘要 |
Steel for forging having high strength and superior machinability due to controlled cooling immediately after shaping by hot forging followed by tempering and having a lower specific gravity than ordinary steel for forging use, the steel containing C: 0.05 to 0.50%, Si: 0.01 to 1.50%, Mn: 3.0 to 7.0%, P: 0.001 to 0.050%, S: 0.020 to 0.200%, Al: 3.0 to 6.0%, Cr: 0.01 to 1.00%, and N: 0.0040 to 0.0200% and having a balance of Fe and unavoidable impurities. |