摘要 |
There is provided a material having an excellent conductivity and oxidation resistance as well as a sufficient hardness for probe pins. The present invention provides a probe pin material including Au, Ag, Pd and Cu, wherein the concentration of Au is 40 to 55% by weight, the concentration of Ag is 15 to 30% by weight and the total concentration of Pd and Cu is 15 to 40% by weight. This material can further include 0.6 to 5% by weight of any one element from among Ni, Zn and Co. Furthermore, this alloy can be precipitation-hardened by being heated at 300 to 500°C, enabling provision of a material having a higher hardness. |