发明名称 DIRECT COUPLING OF MELT POLYMERIZATION AND SOLID STATE PROCESSING FOR PET
摘要 <p>Strands of molten polyethylene terephthalate (PET) from a PET polycondensation reactor are solidified, pelletized, and cooled only to a temperature in the range of 50° C. to a temperature near the polymer Tg by contact with water. The still hot pellets are conveyed, optionally followed by drying to remove water, to a PET crystallizer. By avoiding cooling the amorphous pellets to room temperature with water and cool air, significant savings of energy are realized.</p>
申请公布号 EP1675713(B1) 申请公布日期 2013.10.02
申请号 EP20040781853 申请日期 2004.08.23
申请人 GRUPO PETROTEMEX, S.A. DE C.V. 发明人 BONNER, RICHARD, GILL
分类号 B29B9/12;B29B9/06;B29B9/16 主分类号 B29B9/12