摘要 |
A method for making armor plate that is resistant to armor piercing small arms ammunition is provided. The armor plate includes a steel plate having a nominal chemical composition in weight percent of 0.4C-1.8Ni-0.8Cr-0.25Mo. The steel plate is carburized on one side and produces a carburized side and a non-carburized side. The carburized side of the steel plate has a carbon concentration of at least 0.9% by weight and the non-carburized side has a carbon concentration of between 0.38 and 0.45% by weight. After the steel plate has been carburized, it is subsequently thermally processed such that the carburized side has a hardness of at least 58 Rockwell Hardness C (HRC), and the non-carburized side has a hardness of between >=50 and <=55 HRC.
|