<p>The present invention is a method for manufacturing a mixed crystal. The mixed crystal includes either or both of a microcrystal containing selenium and a microcrystal containing sulfur, a microcrystal containing copper, a microcrystal containing zinc, and a microcrystal containing tin. The manufacturing method for the microcrystal includes a step for preparing a mixed liquid in which a mixed liquid that includes either or both of selenium ions and sulfur ions, copper ions, zinc ions, and tin ions is prepared and an electrocrystallization step in which a voltage is applied to the mixed liquid, and the mixed crystal is electro-crystallized.</p> |