发明名称 COPPER ALLOY
摘要 PROBLEM TO BE SOLVED: To provide a copper alloy sheet excellent in strength, conductivity and bending workability.SOLUTION: A copper alloy contains 0.10-0.50% Cr, 0.010-0.30% Ti, 0.01-0.10% Si, and the balance being copper and inevitable impurities, wherein a mass ratio of the Cr content and the Ti content satisfies the relation: 1.0&le;(Cr/Ti)&le;30, a mass ratio of the Cr content and the Si content satisfies the relation: 3.0&le;(Cr/Si)&le;30. When crystal orientation of the copper alloy is measured by an FESEM-EBSP method, the copper alloy has an aggregate texture having the total average area ratio in Brass orientation {011}<211>, S orientation {123}<634>, and Copper orientation {112}<111> of 40-70%.
申请公布号 JP2013173988(A) 申请公布日期 2013.09.05
申请号 JP20120039366 申请日期 2012.02.24
申请人 KOBE STEEL LTD 发明人 SHISHIDO HISAO;TANAKA TOMOMI;SUMINO YUYA;FUGONO AKIRA
分类号 C22C9/00;C22C9/01;C22C9/02;C22C9/04;C22C9/06;C22C9/10;C22F1/00;C22F1/08;H01B1/02 主分类号 C22C9/00