摘要 |
FIELD: metallurgy.SUBSTANCE: alloy contains, wt %: 3.5-4.5 zinc, 3.5-4.5 magnesium, 0.6-1.0 copper, 2.0-3.0 nickel, 0.25-0.3 zirconium, aluminium - balance, at the same time after strengthening thermal treatment the alloy has yield point of 570 MPa, strength limit of 600 MPa, hardness of 160 HY, and after deformation at 440-480°C with speed of 0.001-0.01 1/s the alloy has elongation of more than 500%.EFFECT: production of alloy with equiaxial homogeneous fine-grain structure.4 ex |