FIELD: electricity.SUBSTANCE: steel wire is aluminised during 1-3 cycles, and each cycle consists of heating of steel wire up to temperature of 900°C in shielding atmosphere to the depth of aluminium to steel, submerging to the bath with molten aluminium and intensive cooling up temperature of 550°C after treatment by molten aluminium and the latter is covered by a layer of molten cryolite in order to prevent oxidation of molten aluminium.EFFECT: corrosion resistivity of the wire. |
申请公布号 |
RU2490740(C2) |
申请公布日期 |
2013.08.20 |
申请号 |
RU20100110078 |
申请日期 |
2010.03.17 |
申请人 |
FEDERAL'NOE GOSUDARSTVENNOE OBRAZOVATEL'NOE UCHREZHDENIE VYSSHEGO PROFESSIONAL'NOGO OBRAZOVANIJA JAROSLAVSKAJA GOSUDARSTVENNAJA SEL'SKOKHOZJAJSTVENNAJA AKADEMIJA |
发明人 |
ALOV VIKTOR ANATOL'EVICH;VORONIN ALEKSEJ SERGEEVICH;MESHKOV ALEKSANDR VADIMOVICH;ORLOV PAVEL SERGEEVICH;SOTSKAJA ELIZAVETA VALER'EVNA |
分类号 |
H01B5/02 |
主分类号 |
H01B5/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|