A method for forming structural equipment employed in sulfur containing environments such as oil refineries and the like. In one embodiment, the method comprises: providing a steel composition containing up to 0.35% of C, 0.30 to 3.5% Si, up to 1.2 % Mo, up to 1.35 % Mn, up to 5% Al, less than 12.0 % Cr, balance of Fe and unavoidable impurities; forming a structural component conforming to prevailing industry standards with respect to design, fabrication, inspection and testing, metallurgical and mechanical properties. The structural equipment has a corrosion rate of less than 15 mpy. In one embodiment, the equipment is formed from a steel composition has a carbon equivalent of less than 0.63, requiring no post weld heat treatment ("PWHT"). In another embodiment, the CE is less than 0.45, requiring no preheat nor PWHT. |