发明名称 |
METHOD FOR PRODUCING AN ENGINE COMPONENT, AND ENGINE COMPONENT |
摘要 |
The present application relates to a method for the production of an engine component, in particular a piston for an internal combustion engine, in which an aluminum alloy is cast in a diecasting process. The aluminum alloy comprises the following alloy elements: silicon: 11 to 14.5 % by weight, nickel: 1.7 to 3.5 % by weight, copper: 3.7 to 5.2 % by weight, magnesium: 1.6 to 3.5 % by weight, iron: 0.6 to 1.5 % by weight, manganese: 0.2 to 0.4 % by weight, zirconium: 0.04 to 0.1 % by weight, vanadium: 0.04 to 0.1 % by weight, the aluminum alloy otherwise comprising aluminum and unavoidable contaminants. |
申请公布号 |
WO2013050464(A3) |
申请公布日期 |
2013.07.18 |
申请号 |
WO2012EP69611 |
申请日期 |
2012.10.04 |
申请人 |
FEDERAL-MOGUL NUERNBERG GMBH |
发明人 |
MORGENSTERN, ROMAN;KNOBLOCH, HOLGER;GOEKEN, MATHIAS;HOEPPEL, HEINZ WERNER;KORN, MATTHIAS;BECK, TILMANN;HUMBERTJEAN, ALEXANDER |
分类号 |
F16J1/00;C22C21/02 |
主分类号 |
F16J1/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|