摘要 |
PROBLEM TO BE SOLVED: To provide a propylene polymer molded article having high tensile elongation and scratch resistance, and to provide a propylene polymer composition giving such a molded article.SOLUTION: This propylene polymer composition includes the following propylene polymer (A-1) or propylene polymer (A-2), the following propylene polymer (B) and a nucleating agent. The [propylene polymer(A-1)] is a polymer with intrinsic viscosity measured in tetralin at 135°C of 1.2 dL/g or more but less than 1.7 dL/g. The [propylene polymer(A-2)] is a polymer with intrinsic viscosity measured in tetralin at 135°C of 1.7 dL/g or more and 2.9 dL/g or less. The [propylene polymer(B)] is a polymer with intrinsic viscosity measured in tetralin at 135°C of 0.5 dL/g or more but less than 1.1 dL/g. |