发明名称 PRECURSOR, PROCESS FOR PRODUCTION OF PRECURSOR, PROCESS FOR PRODUCTION OF ACTIVE MATERIAL, AND LITHIUM ION SECONDARY BATTERY
摘要 Active material is obtained by sintering a precursor, has a layered structure and is represented by the following formula (1). The temperature at which the precursor becomes a layered structure compound in its sintering in atmospheric air is 450° C. or less. Alternatively, the endothermic peak temperature of the precursor when its temperature is increased from 300° C. to 800° C. in its differential thermal analysis in the atmospheric air is 550° C. or less. LiyNiaCobMncMdOxFz(1) In formula (1), the element M is at least one of Al, Si, Zr, Ti, Fe, Mg, Nb, Ba, and V and 1.9@(a+b+c+d+y)@2.1, 1.0@y@1.3, 0<a@0.3, 0@b@0.25, 0.3@c@0.7, 0@d@0.1, 1.9@(x+z)@2.0, and 0@z@0.15 are satisfied.
申请公布号 US2013168599(A1) 申请公布日期 2013.07.04
申请号 US201113814593 申请日期 2011.07.19
申请人 KATO TOMOHIKO;SANO ATSUSHI;SOBU MASAKI;NOJIMA AKINOBU;KAGAYA YASUNAGA;TDK CORPORATION 发明人 KATO TOMOHIKO;SANO ATSUSHI;SOBU MASAKI;NOJIMA AKINOBU;KAGAYA YASUNAGA
分类号 H01M4/1315 主分类号 H01M4/1315
代理机构 代理人
主权项
地址