发明名称 |
AMORPHOUS ALUMINUM SILICATE SALT MANUFACTURING METHOD, ALUMINUM SILICATE SALT OBTAINED WITH SAID METHOD, AND ADSORPTION AGENT USING SAME |
摘要 |
The present invention aims to provide an adsorbent with superior adsorption performance of 20 wt% or more in a humidity range of 5 to 60 wt% by using a low-cost reagent as the raw material. Aluminum sulfate is used as the Al source, the respective aqueous solutions are mixed to achieve a Si/Al molar ratio of 0.70 to 1.0 in the mixed solution, the pH is adjusted to be 6 to 9 with acid or alkali, the solution is heated at 90 to 110°C and subsequently subject to desalination treatment in order to synthesize an amorphous aluminum silicate. The obtained amorphous aluminum silicate yields a superior water vapor adsorption performance of 20 wt% or more in a relative humidity of 60%, and can be used as an adsorbent for desiccant air conditioning and as other adsorbents. |
申请公布号 |
EP2322479(A4) |
申请公布日期 |
2013.07.03 |
申请号 |
EP20090811500 |
申请日期 |
2009.09.02 |
申请人 |
NATIONAL INSTITUTE OF ADVANCED INDUSTRIAL SCIENCEAND TECHNOLOGY |
发明人 |
SUZUKI MASAYA;TSUKIMURA KATSUHIRO;INUKAI KEIICHI;KOZUKA NATSUKO;MAEDA MASAKI |
分类号 |
C01B33/26;B01D53/28;B01J20/16;F24F3/14 |
主分类号 |
C01B33/26 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|