摘要 |
<p>To provide a sealing material which is excellent in sealability under high-temperature conditions as well as crack resistance at high temperatures and high compression. A sealing material comprising
a cross-linked fluororubber layer obtainable by cross-linking a fluororubber composition containing a fluororubber (A) and a carbon black (B),
the cross-linked fluororubber layer having a loss modulus E" of 600 kPa or higher and 6,000 kPa or lower determined by a dynamic viscoelasticity test under conditions of measurement temperature: 160°C, tensile strain: 1%, initial force: 157 cN, and frequency: 10 Hz.</p> |
申请人 |
DAIKIN INDUSTRIES, LTD. |
发明人 |
TERADA JUNPEI;OTA, DAISUKE;KITAICHI, MASANORI;UETA, YUTAKA;MORITA, SHIGERU;KAWASAKI, KAZUYOSHI;MORIKAWA, TATSUYA;FUKUOKA, SHOJI |