摘要 |
A thermoplastic resin composition includes (A) a transparent rubber modified aromatic vinyl copolymer including (a1) a graft copolymer including a core of a rubber based polymer and a shell formed on a surface of the core by graft polymerization of alkyl ester monomer, unsaturated nitrile monomer, and aromatic vinyl monomer; and (a2) a non-graft copolymer including a unit derived from an alkyl ester monomer; and (B) a low molecular weight acrylic copolymer with a weight average molecular weight of about 1,000 to about 10,000 g/mol. The thermoplastic resin composition can have a melt flow index of about 13 to about 35 g/10 min, a haze of about 2 to about 5%, and a Notch Izod impact strength of about 11 to about 15 kgf·cm/cm.
|