发明名称 SECONDARY BATTERY
摘要 A porosity X of a positive electrode mixture layer 223 of a secondary battery 100 is 30(%)≦̸X. A mass ratio α of a positive electrode active material 610 in the positive electrode mixture layer 223 is 0.84≦̸α≦̸0.925 and a mass ratio &bgr; of a conductive material 620 in the positive electrode mixture layer 223 is 0.06≦̸&bgr;≦̸0.12. In the secondary battery 100, an index Y worked out from an expression below is 30 (mL/100 g)≦̸Y≦̸89 (mL/100 g). The index Y is given by the expression below, Y=A×α+B×&bgr;; where A is a DBP absorption number (mL/100 g) in the positive electrode active material 610; α is the mass ratio of the positive electrode active material 610 in the positive electrode mixture layer 223; B is a DBP absorption number (mL/100 g) of the conductive material 620; and &bgr; is the mass ratio of the conductive material 620 in the positive electrode mixture layer 223.
申请公布号 KR20130070651(A) 申请公布日期 2013.06.27
申请号 KR20137012215 申请日期 2010.10.15
申请人 TOYOTA JIDOSHA KABUSHIKI KAISHA 发明人 NAGAI HIROKI;MORITA MASAHIRO;IWAO TAKASHI
分类号 H01M4/13;H01M4/139;H01M4/505;H01M10/04 主分类号 H01M4/13
代理机构 代理人
主权项
地址