摘要 |
PURPOSE: A manufacturing method of a porous sintering aggregate for wastewater odor removing and the porous sintering aggregate are provided to remove bad odor of foul water for a long term without maintenance by integrating the bad odor of foul water after removing the same in a short time. CONSTITUTION: A manufacturing method of a porous sintering aggregate(10) for removing foul water bad odor comprises the following steps: forming mixtures(20) by mixing zeolite, loess, bentonite, wood dust, and diatomite; and manufacturing the mixture into the porous sintering aggregate by sintering a molded body with a desired size and forming at 700-1200 deg. Celsius for 1 hour and 30 minutes to 2 hours. The component ratio of the mixture comprises 50-60 parts by weight of loess, 7-10 parts by weight of bentonite, 7-10 parts by weight of zeolite, 7-10 parts by weight of diatomite, and 7-10 parts by weight of wood dust. |