AMORPHOUS IONICALLY-CONDUCTIVE METAL OXIDES, METHOD OF PREPARATION, AND BATTERY
摘要
A method for forming an amorphous ionically conductive metal oxide, such as lithium lanthanum zirconium oxide (LLZO), by chemical vapor deposition (CVD), as well as to the ionically conductive material formed by the method, are provided. Such a material may be utilized as a solid electrolyte and/or as a solid separator in an all solid state lithium battery.
申请公布号
WO2013085557(A1)
申请公布日期
2013.06.13
申请号
WO2012US27545
申请日期
2012.03.02
申请人
JOHNSON IP HOLDING, LLC;JOHNSON, LONNIE G.;BABIC, DAVORIN;KRUMENAKER, ELENA N.;CAMPBELL, TEDRIC D.;CLAFFEY, KIERAN J.
发明人
JOHNSON, LONNIE G.;BABIC, DAVORIN;KRUMENAKER, ELENA N.;CAMPBELL, TEDRIC D.;CLAFFEY, KIERAN J.