发明名称 NiCuZn FERRITE POWDER FOR MICROWAVE ABSORPTION HEATING ELEMENT AND THE MICROWAVE ABSORPTION HEATING ELEMENT USING THE POWDER
摘要 <P>PROBLEM TO BE SOLVED: To provide NiCuZn ferrite powder for a microwave absorption heating element which can optionally select a temperature-rising stop temperature in a wide range of 50-550&deg;C. <P>SOLUTION: The NiCuZn ferrite powder has a predetermined component composition. An average particle size of the NiCuZn ferrite powder is 2-500 &mu;m, and a relationship between the temperature-rising stop temperature Ts (&deg;C) of the NiCuZn ferrite powder and a value &sigma;s<SB POS="POST">1</SB>(emu/g) of saturation magnetization at the temperature-rising stop temperature Ts satisfies the following formula (1): &sigma;s<SB POS="POST">1</SB>&ge;0.06&times;Ts-1.38. <P>COPYRIGHT: (C)2013,JPO&INPIT
申请公布号 JP2013117367(A) 申请公布日期 2013.06.13
申请号 JP20120181854 申请日期 2012.08.20
申请人 JFE CHEMICAL CORP 发明人 NAKAMURA YUKIKO;TAKAHASHI MIKIO;GOTO SATOSHI
分类号 F24C7/02;H01F1/00;H01F1/34;H01F1/36;H05B6/74 主分类号 F24C7/02
代理机构 代理人
主权项
地址