摘要 |
<P>PROBLEM TO BE SOLVED: To provide a resin plate that is light, hardly cracked, and excellent in appearance, an electrode plate and a resistance film type touch panel, and to provide a resin plate obtained by melt extrusion molding, that is light, hardly cracked, small in a retardation value, and excellent in appearance. <P>SOLUTION: The resin plate includes an acrylic resin layer and a polycarbonate resin layer provided on both surfaces of the acrylic resin layer. A ratio (A:C) of an MFR (Melt Flow Rate) at 230°C×37.3 N of an acrylic resin (A) used for the acrylic resin layer to an MFR at 230°C×37.3 N of a polycarbonate resin (C) used for the polycarbonate resin layer is 1:1.3 to 1:5. <P>COPYRIGHT: (C)2013,JPO&INPIT |