摘要 |
<P>PROBLEM TO BE SOLVED: To provide a resin composition high in productivity in an industrial scale and excellent in moldability and draw-down resistance; to provide a molded article excellent in heat resistance, mechanical strength such as impact resistance, and surface appearance; and to provide a method for producing the same. <P>SOLUTION: The method for producing the resin composition is characterized by melt-blending a polyarylene sulfide resin (A) having a carboxy group at the terminals at a rate of 25-45 [μmol/g] in the resin, a non-Newton index of 0.90-1.15, and a melt viscosity of 1,000-3,000 poises measured at 300°C, and a polyolefin (B) having a functional group reacting with the carboxy group, in a rate of 5-30 pts.mass of the epoxy group-containing polyolefin (B) based on 100 pts.mass of the polyarylene sulfide resin (A); and there is provided the molded article using the resin composition. <P>COPYRIGHT: (C)2013,JPO&INPIT |