摘要 |
FIELD: metallurgy.SUBSTANCE: proposed method comprises sulfuric acid leaching of scandium from red mud, pulp filtration, scandium sorption from sulfuric acid solutions, desorption from organic phase by carbonate solution to obtain column effluent. Then, scandium poorly soluble compounds are precipitated from column effluent, precipitate is filtered out, flushed, dried and annealed to get scandium-bearing concentrate. Note here that said leaching is performed by 10.0-13.5%-sulfuric acid at pulp initial vibration cavitation at rotary velocity of 35-60 m/s for 15-35 min. Scandium is precipitated from column effluent by potassium caprinate in amount of 75-100 g/t of scandium at pH 3.5-4.5 and exposure for 15-25 min.EFFECT: increased yield.3 cl, 2 tbl, 2 ex |