摘要 |
A method of forming members of fiber reinforced thermoplastic members via molding, the members including at least one hollow chamber, formed by water injection into the melt in the mold, to stiffen the finished member. The thermoplastic is preferably selected from a group comprising polypropylene, Nylon, PET, ABS, TPO, and thermoplastic polyurethane, while the reinforcing fibers are preferably selected from a group comprising glass, aramid, carbon, and natural fibers. Preferably, the extruded melt is produced such that the average length of the reinforcing fibers is less than four millimeters.
|