发明名称 ANTI-FOGGING THIN FILM
摘要 <P>PROBLEM TO BE SOLVED: To provide a cellulose ester film excellent in operativity, with wrinkles and peeling after adhesion restrained, while maintaining high anti-fogging characteristics. <P>SOLUTION: The anti-fogging cellulose ester film is produced by applying an alkali saponification process to at least one side of a cellulose ester film after formation thereof. It satisfies formula (1): 1.017&le;S(t)/S(r)&le;1.100, wherein S(t) is the dimensional change rate (%) in the film thickness direction when the relative humidity is changed from 20% at 23&deg;C to 80% at 23&deg;C, and S(r) is the dimensional change rate (%) in the film surface direction in changing the relative humidity 20% (23&deg;C) to 80% (23&deg;C). <P>COPYRIGHT: (C)2013,JPO&INPIT
申请公布号 JP2013100401(A) 申请公布日期 2013.05.23
申请号 JP20110244643 申请日期 2011.11.08
申请人 KONICA MINOLTA ADVANCED LAYERS INC 发明人 WATANABE YASUHIRO;UMEDA HIRONORI;KIMURA HIDETO;BEKKU HIROSHI
分类号 C08J7/00;C08J5/18;C08K5/10;C08L1/08 主分类号 C08J7/00