发明名称 Method for arc welding with consumable electrode
摘要 Methods for arc welding unalloyed or low-alloy steels with consumable electrode under protective gas are suggested, in which the protective gas is a mixture comprising at least helium and an active gas as well as a further inert gas. In the general case, the proportion of the active gas in the total volume of the protective gas is to be in the range from more than 0.5% to approximately 1.5% and the proportion of helium in the total volume of the protective gas is to be more than 30%. In case an electrode having a lowered or medium Si content of approximately 0.2% to approximately 0.4% is used, the proportion of the active gas in the total volume of the protective gas is to be approximately 1% to approximately 5%. If an electrode with a low Si content of approximately 0.05% to approximately 0.1% is used, the proportion of the active gas in the total volume of the protective gas is to be approximately 3% to approximately 10%.
申请公布号 US8445808(B2) 申请公布日期 2013.05.21
申请号 US20090609059 申请日期 2009.10.30
申请人 MATZ CHRISTOPH;LINDE AG 发明人 MATZ CHRISTOPH
分类号 B23K9/00 主分类号 B23K9/00
代理机构 代理人
主权项
地址