摘要 |
A thermoplastic composition can comprise: polycarbonate, aromatic sulphone sulphonate, aromatic sulphonate, and brominated polycarbonate. In an embodiment, when the composition is formed into a 3 mm thick extruded sheet, the sheet can have a smoke density of less than 200 at an exposure period of 240 seconds in accordance with the smoke density test as set forth in ASTM E662-06, and a burn length of less than 150 mm, a drip flame time of less than 3 seconds, and an overall flame time of less than 15 seconds in accordance with the flammability test as set forth in 14 C.F.R. 25.853, Appendix F, Part I(a)(1)(ii).
|