摘要 |
<p>The purpose of the present invention is to reduce mould defects such as incomplete filling. At a resin supply part, a base resin part (27a) is formed from a granular resin (27) on a workpiece (W), and a convex resin part (27b) is formed, from a smaller amount of granular resin (27) than was used to form the base resin part (27a), on the base resin part (27a). At a press part (21), an upper mould (43) and a lower mould (44) are brought closer to the workpiece (W) mounted on the lower mould (44), whereby the upper mould (43) is brought into contact with the convex resin part (27b), molten resin is spread out on the base resin part (27a), and a cavity (45) is filled with resin.</p> |