<P>PROBLEM TO BE SOLVED: To provide a fine-grain tin-doped indium oxide particle having high dispersibility. <P>SOLUTION: The tin-doped indium oxide particle is obtained by adding an indium source and a tin source into a solution, wherein hydroxide of a quaternary ammonium ion is dissolved in a reducing organic solvent, to react them, and then, heating the reaction resultant solution inside an autoclave to mature it under an autogenous pressure. A favorable tin-doped indium oxide particle is obtained using tetramethylammonium hydroxide as the hydroxide of the quaternary ammonium ion. <P>COPYRIGHT: (C)2013,JPO&INPIT |