发明名称 BINDER COMPOSITION FOR CONCRETE COMPRISING BOTTOM ASH
摘要 <p>PURPOSE: A binder composition for concrete is provided to include an ash mixture with bottom ash and fly ash, blast furnace slag micropowder, and Portland cement, thereby having excellent chemical resistance, salt resistance, and durability. CONSTITUTION: A binder composition for concrete comprises: 10-30wt% of ash mixture which comprises 5-50wt% of bottom ash and 50-95wt% of fly ash; 30-50wt% of blast furnace slag micropowder; and 30-40wt% of Portland cement. The brain specific surface area of the ash mixture is 6,000-8,000cm^2/g. The ash mixture is manufactured by mechano-chemical treatment in a condition which physical energy of 50-150KJ/s per unit meter(m^3) is applied. The ash mixture is mechano-chemical treated by being pulverized using a mill for 30-120 minutes. Accumulated hydration heat after 3 days is 120-170J/g. [Reference numerals] (AA) Example 1; (BB) Example 2; (CC) Comparative example 1; (DD) Comparative example 2; (EE) Comparative example 3</p>
申请公布号 KR20130048482(A) 申请公布日期 2013.05.10
申请号 KR20110113347 申请日期 2011.11.02
申请人 CONSTRUCTION STANDARD TEST COMPANY 发明人 LEE, JUN WOO
分类号 C04B18/08;C04B18/14;C04B28/04 主分类号 C04B18/08
代理机构 代理人
主权项
地址